this post was submitted on 13 Aug 2023
28 points (96.7% liked)

3DPrinting

15549 readers
218 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

Been using prusaslicers default PLA profile with issues and this is my first roll of PETG, so I just selected the corresponding profile for that.

It seems so be super stringy whenever there’s movement and when printing the bunny (in vase mode) there’s lots of holes in the model.

I’m not sure if this is an issue with calibration (didn’t do anything when switching from PLA) or if the filament is wet.

you are viewing a single comment's thread
view the rest of the comments
[–] SymbioteSynapse@lemmy.world 8 points 1 year ago (1 children)

Check for a partial clog. 80% of the time i get that consistency with petg, its because the nozzle is partially clogged. The other 20% is the ptfe tubing is shot. Usually it partially melts and causes underextrusion.

Wet filament could be an issue too, but this is pretty extreme for wet filament.

[–] drudoo@lemmy.world 1 points 1 year ago (1 children)

You were right! All clogged up.

Replaced the nozzle, heat block (heating element, sensor, PTFE) and fan duct. Wasn’t able to unscrew the nozzle (got stuck 80% out) so I replaced the whole thing.

Did two new temp towers:

Left tower is 235 (top) to 260 (layers labeled 280-260 are all 260). Right is 220-240.

https://i.imgur.com/1MQkStE.jpg

https://i.imgur.com/HDWq19A.jpg

I definitely feel like 220 is the right temp for this.

[–] SymbioteSynapse@lemmy.world 1 points 1 year ago

Make sure you calibrate your e-steps after swapping hotends. I did the same thing on my ender 3 putting on a volcano hotend, and started getting overextrusion. After adjusting the e-steps it was back to normal.