view the rest of the comments
3DPrinting
3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.
The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io
There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml
Rules
-
No bigotry - including racism, sexism, ableism, homophobia, transphobia, or xenophobia. Code of Conduct.
-
Be respectful, especially when disagreeing. Everyone should feel welcome here.
-
No porn (NSFW prints are acceptable but must be marked NSFW)
-
No Ads / Spamming / Guerrilla Marketing
-
Do not create links to reddit
-
If you see an issue please flag it
-
No guns
-
No injury gore posts
If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)
Moderation policy: Light, mostly invisible
Adhesion can be better, but it also acts as a release agent. If you are printing PETG on glass always use glue, for PLA it shouldnt be needed.
I am in deed printing with Pla but it sticks waaaay too well onto the surface
In my experience PLA just pops off the clean glass when cooled to room temp (holds extremely well if bed is at 45C or more). I have some tips, but only to improve adhesion xD You can maybe try less squish on the first layer (lower flow rate or increase nozzle distance a bit) or just use thin layer of glue. Too low or too high bed temp can ruin bed adhesion, but feels like wrong approach imo, still worth a try
glue or hairspray